High activity POP with solid content of 27 is used in preparation of high-load flexible polyurethane foam by mixing with high activity PPG. The hardening capability is higher than POP 36/28, but is less than HPOP 40.

Feature

High activity POP with solid content of 27 is used in preparation of high-load flexible polyurethane foam by mixing with high activity PPG. The hardening capability is higher than POP 36/28, but is less than HPOP 40.

Performance

Hydroxylvalue(mgKOH/g)23-27 Water content(%)≤ 0.05 PH(ph)5-8 Viscosity (mPa·s/25℃)≤3500 solid content(%)26-28 Functionality 3