Go back
Application
"High activity POP with solid content of 40 is used in preparation of high-load flexible polyurethane foam by mixing with high activity PPG. The hardening capability is higher than POP 36/28 and POP93/28.
"
Feature
"High activity POP with solid content of 40 is used in preparation of high-load flexible polyurethane foam by mixing with high activity PPG. The hardening capability is higher than POP 36/28 and POP93/28.
"
Performance
Hydroxylvalue(mgKOH/g)20-23 Water content(%)≤ 0.05 PH(ph)6-9 Viscosity (mPa·s/25℃)≤6500 solid content(%)39-41 Functionality 3
Files